Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 495N - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 495N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Styrolution® PS 495N is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9.5 cm³/10min ISO 1133
Température 200 °C -
Charge 5 kg -
Densité du fondu 935 kg/m³ -
Conductivité thermique du fondu 0.165 W/(m K) -
Chaleur spécifique du fondu 2290 J/(kg K) -
Température d'éjection 88 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2000 MPa ISO 527
Contrainte d'écoulement 26 MPa ISO 527
Déformation au seuil d'écoulement 1.5 % ISO 527
Déformation nominale à la rupture 40 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 130 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 17 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 85 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 89 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 88.5 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 100 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 2.5 - IEC 62631-2-1
Permittivité relative, 1MHz 2.5 - IEC 62631-2-1
Facteur de pertes, 100Hz 4 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 4 E-4 IEC 62631-2-1
Indice de résistance au cheminement 500 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1030 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Styrolution® PS 495N, PS-I, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Styrolution® PS 495N, PS-I, INEOS Styrolution
Contrainte / Déformation , Styrolution® PS 495N, PS-I, INEOS Styrolution
Module sécant / Déformation , Styrolution® PS 495N, PS-I, INEOS Styrolution
Volume spécifique (pvT) , Styrolution® PS 495N, PS-I, INEOS Styrolution
Module de traction / Température , Styrolution® PS 495N, PS-I, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Modifié choc
Disponibilité régionale
Autres informations
Moulages par injection
PROCESSING
injection molding, Melt temperature, range: 180 - 260 °C
injection molding, Melt temperature, recommended: 220 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 495N can be injection moulded under different conditions depending on machinery available and articles moulded. Mass temperature can be as high as 260°C. Polystyrol 495N is suitable for gas assisted injection moulding.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.